Dear Mr Ganeshan,
As per basic welding fundamentals and good engineering practice, any Chrome-bearing steel need to be purged on other side during GTAW welding.
Chromium has greater affinity for oxygen when heated and get oxidized at once, which in turn depletes the chromium content in the grains. The properties of the steel will get badly affected with this chromium depleted material.
Hence, back purging for T91 is must.
Kind Regards,
Nikhil Parikh
QC Engineer, GDP, Sharjah, UAE
+97150 1453525
On Sat, 11 Jul 2009 08:10:01 +0530 wrote
>
>
>Dear Sir,
>
>Plz. any body can help to me.
>
>
>SA 213 T91 (P5B G 2) the mentioned material purging required (or) not required. If required where given in code.
>
>..
>Thanks & Regards,
>
>K.GANESAN
>Quality Control
>ISGEC / ISGEC John Thompson,
>A-4 Sector-24 Noida-201301 (UP)
>Tel. +91-120-2411175
>Direct Tel. +91-120-2411175
>Mobile : +91-9952166894
>
>
> See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz. http://in.buzz.yahoo.com/
>>
>
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
As per basic welding fundamentals and good engineering practice, any Chrome-bearing steel need to be purged on other side during GTAW welding.
Chromium has greater affinity for oxygen when heated and get oxidized at once, which in turn depletes the chromium content in the grains. The properties of the steel will get badly affected with this chromium depleted material.
Hence, back purging for T91 is must.
Kind Regards,
Nikhil Parikh
QC Engineer, GDP, Sharjah, UAE
+97150 1453525
On Sat, 11 Jul 2009 08:10:01 +0530 wrote
>
>
>Dear Sir,
>
>Plz. any body can help to me.
>
>
>SA 213 T91 (P5B G 2) the mentioned material purging required (or) not required. If required where given in code.
>
>..
>Thanks & Regards,
>
>K.GANESAN
>Quality Control
>ISGEC / ISGEC John Thompson,
>A-4 Sector-24 Noida-201301 (UP)
>Tel. +91-120-2411175
>Direct Tel. +91-120-2411175
>Mobile : +91-9952166894
>
>
> See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz. http://in.buzz.yahoo.com/
>>
>
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments