[MW:2621] Re: 2616] Re: QW 407.3

Ref BS 5500 Latest Edition is more clear on the total soaking time etc , while conducting PQR with PWHT.

----- Original Message -----
From: Sujeet Sangle
To: materials-welding@googlegroups.com
Sent: Sat, 4 Jul 2009 12:00:59 +0530 (IST)
Subject: [MW:2619] Re: 2616] Re: QW 407.3

Friends ,

 

i am sujeet new member of the group .

 

Dear Vasanth ,

 

Yes you are right , i have also interpreted it in the same manner .

 

Rgds

 

Sujeet


On Sat, Jul 4, 2009 at 11:51 AM, Chandra, Vasanthan (Lagos) <Vasanthan.Chandra@deltaafrik.com> wrote:




 


I hope the  interpretation of clause is that if the production welding soaking time is X hrs (Includes total soaking time involved in production like intermediate, dehydrogenation, final PWHT etc…) then the supporting PQR soaking time shall be atleast 80% to the X hrs.  WPS can be written with this PQR to cover the Production time X hrs.



 


Regards,


Vasanth


 


 







From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal

Sent: 03 July 2009 08:05
To: materials-welding@googlegroups.com

Subject: [MW:2616] Re: QW 407.3


 






The underlying meaning eludes me; why would one want to increase the soaking time at an additional cost and what not, over and above the WPS allowed one by way of a PQR? Something jinxes.

Shashank Vagal

--- On Tue, 30/6/09, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:




From: PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com>

Subject: [MW:2594] Re: QW 407.3
To: arunvani@gmail.com
Cc: materials-welding@googlegroups.com

Date: Tuesday, 30 June, 2009, 10:15 AM



I think it is QW-407.2 you guys are referring, because QW407.3 does not appear in Sec.IX 2007 edition !

Regards

Prem Nautiyal

On Sun, 28 Jun 2009 19:41:18 +0530 wrote

>you are right, rajagopal
>arun
>
>On Sun, Jun 28, 2009 at 11:28 AM, rajagopal kannan <
>rajagopal.kannan@gmail.com> wrote:

>
>> Hi,
>> That is if you do heat treatment of your PQR Test coupon to 80 minutes
>> soaking time, then you can write a WPS for production welds to the maximum
>> of 100 minutes soaking time.

>> Thanks,
>> K.Rajagopal
>>
>>   On 6/27/09, Jamie Welding wrote:
>>>
>>>
>>> Hi folks,
>>> Can any one of u interpret the QW 407.3.
>>> Especially the part PQR should be at least 80% aggregate times that in

>>> production welds.
>>> >>
>>>
>
>
>--
>ARUNVANI
>
>Smiling Opens the Heart
>
>Good feelings for others are like ointments that heal wounds and

>re-establish friendships and relationships. Good feelings are generated in
>the mind, are transmitted through your attitude and are reflected in your
>eyes and smile. Smiling opens the heart and a glance can make miracles

>happen.
>
>SMILE IS A COOLING SYSTEM OF HEART,
>SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF
>MIND....
>SO TO ACTIVATE ALL YOUR SYSTEM
>==ALWAYS KEEP SMILING==

>
>>
>

PREM S NAUTIYAL

CELL : 9820313278



















Yahoo! recommends that you upgrade to the new and safer Internet Explorer 8

*** WORLEYPARSONS GROUP NOTICE *** 
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."



--
Click for exclusive coverage on the Maruti Ritz by ZigWheels.com experts
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Blog Archive