Hi!
As per QW 409.1 There is no tolerance for increase in heat input but you can reduce heat input.. Increase in heat input calls for requalification of PQR
Regards
Hegde
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Huub de Goey
Sent: Monday, June 08, 2009 2:19 PM
To: materials-welding@googlegroups.com
Subject: [MW:2351] Re: Heat Input formula
Hi
The first statement is correct.
However, please keep in mind that you cannot guarantee that you're fullfilling logical requirements (range +/- 25% of PQR value)
Allways state on WPS's something like:
Corresponding with the welding in practice, the min Amp level+ the min Volt level are to be used with tje min speed level
the max Amp level+ the max Volt level are to be used with tje max speed level.
Regards,
Huub de Goey2009/6/8 Chandra, Vasanthan (Lagos) <Vasanthan.Chandra@deltaafrik.com>
Friends,
I have got the following formulae for calculating the heat input for SMAW and other welding processes'. Pl confirm which one is correct. As far as I am concerned, I am following the FIRST SET for all the process.
First Set:
- Max Amp x Max V / Min Speed : Max Heat Input
- Min Amp x Min V / Max Speed : Min Heat Input
Second Set:
- Max Amp x Max V / Max Speed : Max Heat Input
- Min Amp x Min V / Min Speed : Min Heat Input
Third set:
- Min Amp x Max Volts /Min Speed : Maximum Heat Input
- Max Amp x Min Volt / Max Speed : Minimum Heat Input
Regards,
Vasanth
*** WORLEYPARSONS GROUP NOTICE ***"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.Any personal views or opinions expressed by the writer may notnecessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
--
Thanks & Regards
Muhammed Ibrahim PK
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com