n't it?
Since you have joined only today, you can't recive the past
discussions, for referring them you might check at http://materials-welding.blogspot.com/
or http://groups.google.com/group/materials-welding?hl=en
On Jun 8, 1:26 pm, "M Zulfan Syahrian" <z.syahr...@gmail.com> wrote:
> All,
>
> anyone can advice me why i can't recieve whoever was sending email to material-welding,while i have subscribe in this group
>
> Rgds
> zulfan
>
>
>
> ----- Original Message -----
> From: handry gmail
> To: z.syahr...@gmail.com
> Sent: Monday, June 08, 2009 2:01 PM
> Subject: Fw: [MW:2345] Heat Input formula
>
> ----- Original Message -----
> From: Chandra, Vasanthan (Lagos)
> To: materials-welding@googlegroups.com
> Sent: Monday, June 08, 2009 1:55 PM
> Subject: [MW:2345] Heat Input formula
>
> Friends,
>
> I have got the following formulae for calculating the heat input for SMAW and other welding processes'. Pl confirm which one is correct. As far as I am concerned, I am following the FIRST SET for all the process.
>
> First Set:
>
> 1.. Max Amp x Max V / Min Speed : Max Heat Input
> 2.. Min Amp x Min V / Max Speed : Min Heat Input
>
> Second Set:
>
> 1.. Max Amp x Max V / Max Speed : Max Heat Input
> 2.. Min Amp x Min V / Min Speed : Min Heat Input
>
> Third set:
>
> 1.. Min Amp x Max Volts /Min Speed : Maximum Heat Input
> 2.. Max Amp x Min Volt / Max Speed : Minimum Heat Input
>
> Regards,
>
> Vasanth
>
> *** WORLEYPARSONS GROUP NOTICE ***
> "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
> If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
> Any personal views or opinions expressed by the writer may not
> necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."- Hide quoted text -
>
> - Show quoted text -
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments