[MW:2350] RE: 2347] RE: 2345] Heat Input formula

 

Hegde Saab,

 

I agree with you. However, as per Sec IX, the heat input can be calculated in either bead length or formula basis. If formula basis, then which one is applicable apart from bead length. Pl give me your input.

 

Regards,

Vasanth

 

 

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PB HEGDE
Sent: 08 June 2009 08:28
To: materials-welding@googlegroups.com
Subject: [MW:2347] RE: 2345] Heat Input formula

 

Friends

i)For SMAW process , The Formula given is a thumb rule but

ii)We generally major on bead length basis ,As we have observed in SMAW ,it is difficult to control the  consistent Current and Voltage

i.e.

Say For 4Dia x 450 length of electrode

We measure  the weld bead length after  burning say 400mm length of electrode  and the same is recorded in PQR/ e.g. 350mm bead length  for burning of 400mm electrodes . This way we control the heat input of weld to get good impact property

We can mention the bead length against individual size electrodes in WPS

 

Regards

 

Hegde p.B.

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandra, Vasanthan (Lagos)
Sent: Monday, June 08, 2009 12:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:2345] Heat Input formula

 

 

Friends,

 

I have got the following formulae for calculating the heat input for SMAW and other welding processes’. Pl confirm which one is correct. As far as I am concerned, I am following the FIRST SET for all the process.

 

First Set:

 

  1. Max Amp x Max V / Min Speed : Max Heat Input
  2. Min Amp x Min V / Max Speed : Min Heat Input

 

Second Set:

 

  1. Max Amp x Max V / Max Speed : Max Heat Input
  2. Min Amp x Min V / Min Speed : Min Heat Input

 

Third set:

 

  1. Min Amp x Max Volts /Min Speed : Maximum Heat Input
  2. Max Amp x Min Volt / Max Speed : Minimum Heat Input

 

 

Regards,

Vasanth

 

*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential.  If you are not the intended recipient, you must not disclose  or  use the  information contained in it.
If you have received this email in error,  please notify us immediately by return email and delete the email and any attachments. 
Any personal views or opinions expressed by the writer may not 
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

 

 


lang=EN-US>

*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential.  If you are not the intended recipient, you must not disclose  or  use the  information contained in it. If you have received this email in error,  please notify us immediately by return email and delete the email and any attachments.  Any personal views or opinions expressed by the writer may not  necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies." 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...