Ali,
Go and read some of the references I sent a little while ago and stop challenging those who know better than you do. You are wrong. I have told you this before.
 
Owen.
----- Original Message -----
Sent: Saturday, June 06, 2009 12:55 PM
Subject: [MW:2335] Re: corrosion

Dear Keyvan
i think for low alloy steel & carbon steel ,the different chemical analysis in haz & weld isn't major to occur chemical cell.

 


From: kayvan alyari <k.alyari@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, June 6, 2009 3:17:06 PM
Subject: [MW:2334] Re: corrosion

Dear Friends,
 
The main cause is formation of electro chemical cell between HAZ & BM especially in interfaces!
 
Yours truely
Keyvan

 
On 6/6/09, Owen Jenkins <owen@osjl.co.uk> wrote:
If you'd like to know a bit more about corrosion associated with welding, you can download the following guide to bimetallic corrosion: http://www.npl.co.uk/upload/pdf/bimetallic_20071105114556.pdf . The NPL website has a number of other useful downloads which may help you, as well as some illustrations of various forms of corrosion associated with welding. In some cases the HAZ is more susceptible to attack, in others it is the weld metal itself. You can also visit the following sites for more information:  Corrosion Clinic http://come.to/corrosion, Corrosion doctors http://www.corrosion-doctors.org/CorrDocs/CDs.htm, NASA's KSC Corrosion Technology Laboratory http://corrosion.ksc.nasa.gov/ .
 
A Google search would have turned up all that lot for you. Worth trying occasionally, as I've remarked before.
 
Regards,
Owen.
----- Original Message -----
Sent: Saturday, June 06, 2009 9:49 AM
Subject: [MW:2331] Re: corrosion

 
Hi,
It's about the grain sizes and intergranular changes because of welding i think
After welding you will see a lot of different sections that are affected by heat differently.
In most applications weld metals have fine grains due to recrystallization and tempering effects of the upper beads
[And so upper sections of the weld metal have bigger grains (because they are less tempered)]
In the fusion line there is a non-complete fusion section (grain structure is like a casting)
After that, in HAZ a highly heated (but no fusion) big grain size section comes near the fusion line
This section is the most risky one. In most cases if corrosion cracking happens it does it here.
This doesn't mean that weld metal behaves more noble than base metal i think. the corrosion is between the weld metal and HAZ
I didn't see anywhere anything certain about the causes of this type of corrosion.
--

Best Regards,

Erhan TURGUT


Ali Asghari yazmış:

hi
why corrosion occure preferentially in haz ,especially fine grain location?
why weld metal noble than base metal?
 
regard advance




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...