I want the advice of senior members to help me out in qualifying a typical welding procedure as per ASME Sec IX.

We want to weld a 800mm dia. SA105 Gr.B (Carbon steel)forging to a 20mm thick SS304L shell (circumferential seam).
Length of both members is @ 2metres.

The solid forging is tapered and is welded to the 20mm thick SS304L with a full penetration joint where the depth of bevel is 18mm and thickness of both members at the joint is 20mm.
The joint is single V. Only final weld LPT required.

Now logically this 800mm dia. forging will have to be preheated to @150 degrees celcius i believe, but what about SS304L.
Our client has strictly told us that SS304L shell shall not be preheated.
The reason being distortion and a wider HAZ, however i believe that preheating to 100/150 degrees celcius will not change the structure of SS304L and hamper mechanical properties - UTS and bend.

Now i have 2 queries:

1)Should we only preheat the CS forging and mention the same on the WPS ?

2)What should be the appropriate preheat temperature and on what location to preheat?

3)On what plate thickness should i qualify the Welding procedure inorder to qualify the base metal thickness range i.e for 800mm dia. forging?

4)Should i qualify the joint on a dissimilar thickness with weld deposition of only 20mm, so what thickness of plates should i select?

Please advice !

Regards

Prem S Nautiyal
Godrej, Mumbai.

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...