Skip to main content

[MW:1972] RE: 1971] Re: WELDER QUALIFICATION

Yes you can weld P8 to P8 with E309  and qualify for SS as per F no , In GTAW F no 6  qualifies for Cs and SS also

 

Hegde P.B

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Friday, April 17, 2009 11:49 AM
To: material welding
Subject: [MW:1971] Re: WELDER QUALIFICATION

 

Mr. Dale Jones
As you said to weld with F5 stainless steel filler material which is needed to weld with matching filler on P8 materials.I would like to add more...i.e. as per QW 423 Alternate Base Materials for welder qualification we can weld P1 materiel also with F5 SS Filler  in order to qualify welder for any particular P8 WPS.
This is economical as well as within limit of code.
Please correct me if my interpretation is wrong
Regards

Bharat B. Gole

 





Date: Thu, 16 Apr 2009 16:26:34 -0700
From: dalejones7978@yahoo.com
Subject: [MW:1970] Re: WELDER QUALIFICATION
To: materials-welding@googlegroups.com

This is correct that the welder can weld on all of these materials but do not ignore the other variables. For example the welder will be restricted to the Fnumber filler material he qualified with. An example is a SMAW qualification. When a welder qualifies on P1 material with a matching F4 SMAW filler he will be qualified to the base material range stated below and with F1-F4 carbon steel filler material. This will not qualify him to weld with F5 stainless steel filler material which is needed to weld with matching filler on P8 materials. The same concept will apply to various other P numberd materials. To fully understand this concept and the other variables that will restrict a welders qualifications, read article 3 and QW-416 in ASME Section 9

Regards,

Dale Jones

--- On Thu, 4/16/09, Muhammed Ibrahim <ibratech@gmail.com> wrote:


From: Muhammed Ibrahim <ibratech@gmail.com>
Subject: [MW:1968] Re: WELDER QUALIFICATION
To: materials-welding@googlegroups.com
Date: Thursday, April 16, 2009, 5:45 AM

 

 

Not only P11. Also P34 & P41 thru P49. The reason is, the skill of the welder required to weld any of these material is same. So he can proove it in any one P No. mentioned .

 

Regards,

Muhammed Ibrahim


 

2009/4/16 gaurav mongia <er.gauravmongia@gmail.com>


IF A WELDER IS QUALIFIED FOR P1 material and in code it is written
that he is qualified upto P11.

i wanna know what will be reason that a welder can do welding on all
material upto P11 instead he is only qualified in P1






 


How fun is this? IMing with Windows Live Messenger just got better.

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...