[MW:1715] Re: Closure/ Tie in joints - NDEs as per B31.3

hi to all,

As i believe after reading your mail it's a TIE-IN between
old and new line,
if it so, please do UT for thickness checking in the old & MT on same
line in bevel and HAZ( you can prefer PT if the thickness of line is
less than 19 mm).


Syed Farhan
Piping Engineer
Hyundai Heavy Industries

On 06/03/2009, VJ V <veevee17@gmail.com> wrote:
>
>
> Hi All,
>
> There are a couple of Tie-in/Closure joints to be welded in the
> project, I am involved right now. No possibility of Leak test/
> Hydrotest for that joint..
>
> Project spec is ASME B31.3(100% RT),and
> I would like to know is there any requirement of UT and cut bevel MT/
> UT,additional to RT specified by the Code for Closure/ Tie in joints.
>
> I couldn't see that requirement(cut bevel MT,UT) in B 31.3......Am I
> right ?
>
> I have done earlier UT,cut bevel MT additional to RT in other
> projects,but that was as per project spec.
>
> Thanks
>
> >
>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---