Hi friends,
 
Please help me in following matter.
 
I need a clarification regarding the impact test requirement for Nozzle weld.
 
Material - SA 516 Gr.70 Normalised (Shell)
               SA333 Gr.6  (Nozzle neck)
               SA350 Gr. LF2 Cl2 (Flange)
 
Shell thickness - 80 mm
Nozzle thickness - 10 mm
MDMT- minus 30 deg.c
Code : ASME Sec. VIII Div. 1
 
Shell to nozzle neck weld - Is it required Impact tested WPS/PQR ?
Nozzle neck to flange weld - Is it required Impact tested WPS/PQR ?
 
As per UCS 66 (1) d. The weded asembly more than 2 component, the individual component thickness and MDMT to be checked. In this case the thickness of groove is higher than nozzle neck. What thickness to be considered?.
 
UCS 66 (1) d. refers the sketches in Sec. VIII to decide minimum thk. it makes confusion.


Thanks & Regards
Muhammed Ibrahim PK



--
Thanks & Regards
Muhammed Ibrahim PK

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...