About the AGFA Structurix films :
 
Film    ASTM
-------------------
D2    special
D3    I
D4    I
D5    I
D7    II
D8    III
 
Regards,
 
T. Buyle
 

 

Tim Buyle | Research Engineer Welding
ArcelorMittal R&D Industry Gent

OCAS NV | Pres. J.F. Kennedylaan 3
9060 Zelzate | Belgium
T +32 (0)9 345 12 93 | F +32 (0)9 345 12 04
tim.buyle@arcelormittal.com | www.ocas.be

 

 



From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mukesh Kumar
Sent: maandag 2 maart 2009 15:04
To: materials-welding@googlegroups.com
Subject: [MW:1688] Re: 1668] Re: Highlights for ASME sec VIII, Div2 (U2) & ASME sec VIII, Div 3 (U3) Code

Hi All,
 
Could you help me in getting the film ASTM class as per film manufacturer.
 
Whether Agfa D7 is ASTM Type Class I or Class II.
 
Regards
Mukesh
Lurgi

********************************************************************************
This message and any attachment are confidential, intended solely for the use of the individual or entity to whom it is addressed and may be protected by professional secrecy or intellectual property rights.
If you have received it by mistake, or are not the named recipient(s), please immediately notify the sender and delete the message. You are hereby notified that any unauthorized use, copying or dissemination of any or all information contained in this message is prohibited.
Arcelormittal shall not be liable for the message if altered, falsified, or in case of error in the recipient.
This message does not constitute any right or commitment for ArcelorMittal except when expressly agreed otherwise in writing in a separate agreement.
********************************************************************************

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...