No such requirement in code (B31.3) for min separation, it always from the client standards or the engineering guidelines issued at the beginning of the project, one such is attached herewith gives some idea, which we have used for one of the project in mid 90’s.

150mm as given below by Mr Nilesh for circumferential welds is normal engineering practice (I think Aramco or UOP standards specify similar requirement) followed by most of the pipe fabricators.

As far as I know PFI ES7 gives min spacing for welded nozzles.

EN 13480-3 also give similar requirement for branch welds (refer fig. 8.4.1-2)

Members pl. share if any other codes gives such requirement.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zameer Mohammed
Sent: Tuesday, February 10, 2009 2:32 PM
To: materials-welding@googlegroups.com
Subject: [MW:1537] Re: minimum length

 

Dear Mr. Nilesh,

 

Could you pls give the reference paragraph in the ASME B 31.3 which mentions this?

 

I heard it shall be 5t or min 300mm for the size of a pup piece. No where in the ASME B 31.3 I could see it mentioned. Correct me if I'm wrong.

 

Thank you,

 

Regards,

 

 

Sabir 

 

On Tue, Feb 10, 2009 at 11:28 AM, nilesh <nilesh_parsekar@yahoo.com> wrote:

Dear Javed,

 

   As per ASME 31.3 it should be 150mm

 Nilesh Parsekar,

 QC CO-ORDINATOR

(Dp Mech,API 510,API 570,AWS-CWI,NDT LEVEL2)

 Belleli Energy

 QATAR



--- On Tue, 2/10/09, Mohammad Javeed <mmubasharjaveed@gmail.com> wrote:

From: Mohammad Javeed <mmubasharjaveed@gmail.com>
Subject: [MW:1534] minimum length
To: materials-welding@googlegroups.com
Date: Tuesday, February 10, 2009, 1:09 AM

 

dear all, have a nice day

can any one tell me what is a  minimum length between two butt joints.( piece of pipe) with reference

thanks with regards

m javed



 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...