DIN | Grade | DIN | Grade | DIN | Grade | DIN | Grade |
1701 | WNi99 | 1654-4 | 19MnB4 | 17230 | 19MnCr5 | 43720 | X18CrN28 |
1702 | Ni99.0 | 1654-4 | 22B2 | 17230 | 43CrMo4 | 43720 | X6CrNiMoTi17122 |
1702 | Ni99.4NiO | 1654-4 | 25CrMo4 | 17230 | 44Cr2 | 43720 | X6CrNiTi1810 |
1702 | Ni99CSi | 1654-4 | 28B2 | 17230 | 48CrMo4 | 46400-1 | V250-35A |
1704 | Sn99.00 | 1654-4 | 28Mn6 | 17230 | 80MoCrV4216 | 46400-1 | V270-35A |
1704 | Sn99.50 | 1654-4 | 30CrNiMo8 | 17230 | Cf54 | 46400-1 | V270-50A |
1704 | Sn99.75 | 1654-4 | 34Cr4 | 17230 | X102CrMo17 | 46400-1 | V290-50A |
1704 | Sn99.90 | 1654-4 | 34CrMo4 | 17230 | X45Cr13 | 46400-1 | V300-35A |
1704 | Sn99.95 | 1654-4 | 34CrNiMo6 | 17230 | X75WCrV1841 | 46400-1 | V310-50A |
1706 | Zn97.5 | 1654-4 | 35B2 | 17230 | X82WMoCrV654 | 46400-1 | V330-35A |
1706 | Zn98.5 | 1654-4 | 37Cr4 | 17230 | X89CrMoV181 | 46400-1 | V330-50A |
1706 | Zn99.5 | 1654-4 | 38Cr2 | 17240 | 21CrMoV57 | 46400-1 | V330-65A |
1706 | Zn99.95 | 1654-4 | 41Cr4 | 17240 | 24CrMo5 | 46400-1 | V350-50A |
1706 | Zn99.99 | 1654-4 | 42CrMo4 | 17240 | 40CrMoV47 | 46400-1 | V350-65A |
1706 | Zn99.995 | 1654-4 | 46Cr2 | 17240 | C35 | 46400-1 | V400-50A |
1707 | L-PbAg25Sn2 | 1654-4 | Cq22 | 17240 | Ck35 | 46400-1 | V400-65A |
1707 | L-PbAg2Sn2 | 1654-4 | Cq35 | 17240 | Cq35 | 46400-1 | V470-50A |
1707 | L-PbAg3 | 1654-4 | Cq45 | 17240 | NiCr20TiAl | 46400-1 | V470-65A |
1707 | L-PbAg5 | 1654-5 | X10Cr13 | 17240 | X19CrMoVNbN111 | 46400-1 | V530-50A |
1707 | L-PbSn12Sb | 1654-5 | X2CrNi1911 | 17240 | X22CrMoV121 | 46400-1 | V530-65A |
1707 | L-PbSn2 | 1654-5 | X2CrNiMoN17133 | 17240 | X8CrNiMoBNb1616 | 46400-1 | V600-50A |
1707 | L-PbSn20Sb3 | 1654-5 | X2CrNiN1810 | 17243 | 10CrMo910 | 46400-1 | V600-65A |
1707 | L-PbSn25Sb | 1654-5 | X3CrNiCu189 | 17243 | 13CrMo44 | 46400-1 | V700-50A |
1707 | L-PbSn30(Sb) | 1654-5 | X5CrNi1812 | 17243 | 14MoV63 | 46400-1 | V700-65A |
1707 | L-PbSn30Sb | 1654-5 | X5CrNiMo17122 | 17243 | 15Mo3 | 46400-1 | V800-50A |
1707 | L-PbSn33(Sb) | 1654-5 | X6Cr17 | 17243 | 17Mn4 | 46400-1 | V800-65A |
1707 | L-PbSn35(Sb) | 1654-5 | X6CrNiMoTi17122 | 17243 | 20Mn5 | 46400-1 | V940-50A |
1707 | L-PbSn35Sb | 1654-5 | X6CrNiTi1810 | 17243 | C22.8 | 46400-1 | V940-65A |
1707 | L-PbSn40 | 1681 | GS-38 | 17243 | X20CrMoV121 | 46400-2 | VH1000-65 |
1707 | L-PbSn40(Sb) | 1681 | GS-45 | 17245 | GS-17CrMo55 | 46400-2 | VH1050-50 |
1707 | L-PbSn40Sb | 1681 | GS-52 | 17245 | GS-17CrMoV511 | 46400-2 | VH1200-65 |
1707 | L-PbSn45(Sb) | 1681 | GS-60 | 17245 | GS-18CrMo910 | 46400-2 | VH660-50 |
1707 | L-PbSn8(Sb) | 1691 | GG-10 | 17245 | GS-22Mo4 | 46400-2 | VH800-65 |
1707 | L-Sn50Pb | 1691 | GG-15 | 17245 | GS-C25 | 46400-2 | VH890-50 |
1707 | L-Sn50Pb(Sb) | 1691 | GG-150HB | 17245 | G-X22CrMoV121 | 46400-3 | VM111-30P |
1707 | L-Sn50PbAg | 1691 | GG-170HB | 17245 | G-X8CrNi12 | 46400-3 | VM111-35N |
1707 | L-Sn50PbCu | 1691 | GG-190HB | 17280 | 10Ni14 | 46400-3 | VM117-30P |
1707 | L-Sn50PbSb | 1691 | GG-20 | 17280 | 11MnNi53 | 46400-3 | VM130-27S |
1707 | L-Sn60Pb | 1691 | GG-220HB | 17280 | 12Ni19 | 46400-3 | VM140-30S |
1707 | L-Sn60Pb(Sb) | 1691 | GG-240HB | 17280 | 13MnNi63 | 46400-3 | VM155-35S |
1707 | L-Sn60PbAg | 1691 | GG-25 | 17280 | 14NiMn6 | 46400-3 | VM89-27N |
1707 | L-Sn60PbCu | 1691 | GG-260HB | 17280 | 26CrMo4 | 46400-3 | VM97-30N |
1707 | L-Sn60PbCu2 | 1691 | GG-30 | 17280 | X7NiMo6 | 46400-4 | VE340-50 |
1707 | L-Sn63Pb | 1691 | GG-35 | 17280 | X8Ni9 | 46400-4 | VE390-50 |
1707 | L-Sn63PbAg | 1692 | GTS-35-10 | 17350 | 100Cr6 | 46400-4 | VE390-65 |
1707 | L-Sn70Pb | 1692 | GTS-45-06 | 17350 | 105WCr6 | 46400-4 | VE450-50 |
1707 | L-Sn90Pb | 1692 | GTS-55-04 | 17350 | 110WCrV5 | 46400-4 | VE450-65 |
1707 | L-SnAg5 | 1692 | GTS-65--02 | 17350 | 115CrV3 | 46400-4 | VE520-65 |
1707 | L-SnCd20 | 1692 | GTS-70-02 | 17350 | 145V33 | 46400-4 | VE560-50 |
1707 | L-SnIn50 | 1692 | GTW-35-04 | 17350 | 21MnCr5 | 46400-4 | VE630-65 |
1707 | L-SnPbCd18 | 1692 | GTW-40-05 | 17350 | 31CrV3 | 488-1 | BSt42/50RK |
1707 | L-SnSb5 | 1692 | GTW-40-07 | 17350 | 40CrMnMoS86 | 488-1 | BSt42/50RU |
1707 | L-ZnSn20 | 1692 | GTW-S-38-12 | 17350 | 45CrMoV7 | 488-1 | BSt420S |
1712-1 | Al99.5H | 1693-1 | GGG-35.3 | 17350 | 48CrMoV67 | 488-1 | BSt500G |
1712-1 | Al99.7H | 1693-1 | GGG-40 | 17350 | 51CrV4 | 488-1 | BSt500M |
1712-1 | Al99.8H | 1693-1 | GGG-40.3 | 17350 | 55NiCrMoV6 | 488-1 | BSt500P |
1712-1 | Al99.99R | 1693-1 | GGG-50 | 17350 | 56NiCrMoV7 | 488-1 | BSt500S |
1712-1 | Al99.9H | 1693-1 | GGG-60 | 17350 | 60MnSiCr4 | 536-1 | A100 |
1712-1 | E-AlH | 1693-1 | GGG-70 | 17350 | 60WCrV7 | 536-1 | A120 |
1712-3 | Al99 | 1693-1 | GGG-80 | 17350 | 62SiMnCr4 | 536-1 | A150 |
1712-3 | Al99.0 | 1693-2 | GGG-40 | 17350 | 75Cr1 | 536-1 | A45 |
1712-3 | Al99.5 | 1693-2 | GGG-40.3 | 17350 | 80CrV2 | 536-1 | A55 |
1712-3 | Al99.7 | 1693-2 | GGG-50 | 17350 | 90MnCrV8 | 536-1 | A65 |
1712-3 | Al99.8 | 1693-2 | GGG-60 | 17350 | C105W1 | 536-1 | A75 |
1712-3 | Al99.9 | 1693-2 | GGG-70 | 17350 | C45W | 536-2 | F100 |
1712-3 | Al99.98R | 1694 | GGG-Ni22 | 17350 | C60W | 536-2 | F120 |
1712-3 | E-Al | 1694 | GGG-Ni35 | 17350 | C70W2 | 5512-1 | QSt37-3 |
1719 | Pb98.5 | 1694 | GGG-NiCr202 | 17350 | C80W1 | 5512-1 | QSt52-3 |
1719 | Pb99.75 | 1694 | GGG-NiCr203 | 17350 | C85W | 5512-1 | QSt52-3Cu3 |
1719 | Pb99.94 | 1694 | GGG-NiCr301 | 17350 | S10-4-3-10 | 5512-1 | RQSt37-2 |
1719 | Pb99.985 | 1694 | GGG-NiCr303 | 17350 | S12-1-4-5 | 5512-1 | RQSt37-2Cu3 |
1719 | Pb99.99 | 1694 | GGG-NiCr353 | 17350 | S18-1-2-5 | 5512-1 | RSt37-2 |
1719 | Pb99.9Cu | 1694 | GGG-NiCrNb202 | 17350 | S2-10-1-8 | 5512-1 | RSt37-2Cu3 |
1725-1 | Al99.85Mg0.5 | 1694 | GGG-NiMn137 | 17350 | S2-9-2 | 5512-1 | St33 |
1725-1 | Al99.85Mg1 | 1694 | GGG-NiMn234 | 17350 | S3-3-2 | 5512-1 | St37-3N |
1725-1 | Al99.85MgSi | 1694 | GGG-NiSiCr2052 | 17350 | S6-5-2 | 5512-1 | St50-2 |
1725-1 | Al99.8ZnMg | 1694 | GGG-NiSiCr3052 | 17350 | S6-5-2-5 | 5512-1 | St52-3 |
1725-1 | Al99.9Mg0.5 | 1694 | GGG-NiSiCr3055 | 17350 | S6-5-2-5S | 5512-1 | St52-3Cu3 |
1725-1 | Al99.9Mg1 | 1694 | GGG-NiSiCr3552 | 17350 | S6-5-2S | 5512-1 | St60-2 |
1725-1 | Al99.9MgSi | 1694 | GGL-NiCr202 | 17350 | S6-5-3 | 5512-1 | UQSt37-2 |
1725-1 | AlCu2.5Mg0.5 | 1694 | GGL-NiCr203 | 17350 | S7-4-2-5 | 5512-1 | UQSt37-2Cu3 |
1725-1 | AlCu2Mg0.5 | 1694 | GGL-NiCr303 | 17350 | SC6-5-2 | 5512-2 | St12 |
1725-1 | AlCuBiPb | 1694 | GGL-NiCuCr1562 | 17350 | SC6-5-2S | 5512-2 | St12Cu3 |
1725-1 | AlCuMg1 | 1694 | GGL-NiCuCr1563 | 17350 | X155CrVMo121 | 5512-2 | St14 |
1725-1 | AlCuMg2 | 1694 | GGL-NiMn137 | 17350 | X165CrMoV12 | 5512-2 | St14Cu3 |
1725-1 | AlCuMgPb | 1694 | GGL-NiSiCr2053 | 17350 | X19NiCrMo4 | 5512-2 | St37-2Cu3G |
1725-1 | AlCuSiMn | 1694 | GGL-NiSiCr3055 | 17350 | X210Cr12 | 5512-2 | St37-2G |
1725-1 | AlFeSi | 1695 | G-X260Cr27 | 17350 | X210CrW12 | 5512-2 | St52-3Cu3G |
1725-1 | AlMe2.7Mn | 1695 | G-X260CrMoNi20-2-1 | 17350 | X32CrMoV33 | 5512-2 | St52-3G |
1725-1 | AlMg0.5Mg0.5 | 1695 | G-X260NiCr4-2 | 17350 | X36CrMo17 | 5512-3 | X2Cr11 |
1725-1 | AlMg1 | 1695 | G-X300CrMo15-3 | 17350 | X38CrMoV51 | 5512-3 | X2CrNiN187 |
1725-1 | AlMg1.5 | 1695 | G-X300CrMo27-1 | 17350 | X40CrMoV51 | 5512-3 | X5CrNi1810 |
1725-1 | AlMg1.8 | 1695 | G-X300CrMoNi15-2-1 | 17350 | X45NiCrMo4 | 5512-3 | X5CrNiMo17122 |
1725-1 | AlMg2.5 | 1695 | G-X300CrNiSi9-5-2 | 17350 | X96CrMoV12 | 5512-3 | X5CrNiMoTi152 |
1725-1 | AlMg2.7Mn | 1695 | G-X300NiMo3Mg | 1736-1 | EL-NiCr15FeMn | 5512-3 | X6Cr17 |
1725-1 | AlMg2Mn0.3 | 1695 | G-X330NiCr4-2 | 1736-1 | EL-NiCr15FeNb | 5512-3 | X6CrNiMoTi17122 |
1725-1 | AlMg2Mn0.8 | 17103 | StE285 | 1736-1 | EL-NiCr15MoNb | 5512-3 | X6CrNiTi1810 |
1725-1 | AlMg3 | 17103 | StE355 | 1736-1 | EL-NiCr16FeMn | 5512-3 | X6CrTi12 |
1725-1 | AlMg4.5 | 17103 | StE420 | 1736-1 | EL-NiCr19Mo15 | 59470 | CrAl205 |
1725-1 | AlMg4.5Mn | 17103 | StE460 | 1736-1 | EL-NiCr19Nb | 59470 | CrAl255 |
1725-1 | AlMg4Mn | 17103 | StE500 | 1736-1 | EL-NiCr20Mo9Nb | 59470 | CrNi2520 |
1725-1 | AlMg5 | 17103 | TStE285 | 1736-1 | EL-NiCr21Co12Mo | 59470 | NiCr3020 |
1725-1 | AlMg5Mn | 17103 | TStE355 | 1736-1 | EL-NiCr26Mo | 59470 | NiCr6015 |
1725-1 | AlMgSi0.5 | 17103 | TStE420 | 1736-1 | EL-NiCr28Mo | 59470 | NiCr8020 |
1725-1 | AlMgSi0.7 | 17103 | TStE460 | 1736-1 | EL-NiCu30Mn | 8556-1 | 13 |
1725-1 | AlMgSi0.8 | 17103 | TStE500 | 1736-1 | EL-NiMo15Cr15Ti | 8556-1 | 131 |
1725-1 | AlMgSi1 | 17103 | WStE285 | 1736-1 | EL-NiMo15Cr15W | 8556-1 | 134 |
1725-1 | AlMgSi1Cu | 17103 | WStE355 | 1736-1 | EL-NiMo29 | 8556-1 | 1682 |
1725-1 | AlMgSiPb | 17103 | WStE420 | 1736-1 | EL-NiTi3 | 8556-1 | 17 |
1725-1 | AlMn0.5Mg0.5 | 17103 | WStE460 | 1736-1 | SG-NiCr19NbMoTi | 8556-1 | 17Mo |
1725-1 | AlMn0.6 | 17103 | WStE500 | 1736-1 | SG-NiCr20 | 8556-1 | 18153L |
1725-1 | AlMn1 | 17111 | R10S10 | 1736-1 | SG-NiCr20Mo15 | 8556-1 | 18165L |
1725-1 | AlMn1Mg0.5 | 17111 | R7S6 | 1736-1 | SG-NiCr20Nb | 8556-1 | 1836 |
1725-1 | AlMn1Mg1 | 17111 | RSt36 | 1736-1 | SG-NiCr21Mo9Nb | 8556-1 | 188Mn |
1725-1 | AlMnCu | 17111 | RSt38 | 1736-1 | SG-NiCr22Co12Mo | 8556-1 | 189MnMo |
1725-1 | AlRMg0.5 | 17111 | U10S10 | 1736-1 | SG-NiCr23Al | 8556-1 | 19122 |
1725-1 | AlRMg1 | 17111 | U7S6 | 1736-1 | SG-NiCr27Mo | 8556-1 | 19123 |
1725-1 | AlZn1 | 17111 | UQSt36 | 1736-1 | SG-NiCr29Mo | 8556-1 | 19123L |
1725-1 | AlZn4.5Mg1 | 17111 | UQSt38 | 1736-1 | SG-NiCu30Al | 8556-1 | 19123Nb |
1725-1 | AlZnMgCu0.5 | 17111 | USt36 | 1736-1 | SG-NiCu30MnTi | 8556-1 | 19134L |
1725-1 | AlZnMgCu1.5 | 17111 | USt38 | 1736-1 | SG-NiMo16Cr16Ti | 8556-1 | 199 |
1725-1 | E-AlMgSi | 17115 | 15Mn3Al | 1736-1 | SG-NiMo16Cr16W | 8556-1 | 199H |
1725-1 | E-AlMgSi0.5 | 17115 | 20NiCrMo2 | 1736-1 | SG-NiMo27 | 8556-1 | 199L |
1725-1 | G-AlCu4Ti | 17115 | 20NiCrMo3 | 1736-1 | SG-NiTi4 | 8556-1 | 199Nb |
1725-1 | G-AlCu4TiMg | 17115 | 21Mn4Al | 1736-1 | UP-NiCr20Nb | 8556-1 | 20103 |
1725-1 | G-AlMg3 | 17115 | 21Mn5 | 1736-1 | UP-NiCr21Mo9Nb | 8556-1 | 20163MnL |
1725-1 | G-AlMg3Si | 17115 | 23MnNiCrMo52 | 1736-1 | UP-NiCr22Co12Mo | 8556-1 | 20255CuL |
1725-1 | G-AlMg3Siwa | 17115 | 23MnNiCrMo53 | 1736-1 | UP-NiCu30MnTi | 8556-1 | 20255LCu |
1725-1 | G-AlMg5 | 17115 | 23MnNiMoCr54 | 1736-1 | UP-NiTi4 | 8556-1 | 2212 |
1725-1 | G-AlMg5Si | 17115 | 27MnSi5 | 17405 | Ni48 | 8556-1 | 2293L |
1725-1 | G-AlSi10Mg | 17115 | RSt35-2 | 17405 | RFe100 | 8556-1 | 23122L |
1725-1 | G-AlSi10Mg(Cu) | 17115 | USt35-2 | 17405 | RFe12 | 8556-1 | 2312L |
1725-1 | G-AlSi10Mgwa | 17119 | RSt37-2 | 17405 | RFe120 | 8556-1 | 2312Nb |
1725-1 | G-AlSi11 | 17119 | St37-3 | 17405 | RFe160 | 8556-1 | 23132 |
1725-1 | G-AlSi12 | 17119 | St44-2 | 17405 | RFe20 | 8556-1 | 2520 |
1725-1 | G-AlSi12(Cu) | 17119 | St44-3 | 17405 | RFe60 | 8556-1 | 2520H |
1725-1 | G-AlSi12CuNiMg | 17119 | St52-3 | 17405 | RFe80 | 8556-1 | 25222L |
1725-1 | G-AlSi5Mg | 17119 | USt37-2 | 17405 | RNi12 | 8556-1 | 254 |
1725-1 | G-AlSi6Cu4 | 17119 | WTSt37-2 | 17405 | RNi24 | 8556-1 | 2572 |
1725-1 | G-AlSi7Mg | 17119 | WTSt37-3 | 17405 | RNi8 | 8556-1 | 2593CuL |
1725-1 | G-AlSi9Cu3 | 17119 | WTSt52-3 | 17405 | RSi12 | 8556-1 | 2594L |
1725-1 | G-AlSi9Mg | 17120 | RSt37-2 | 17405 | RSi24 | 8556-1 | 27314CuL |
1725-1 | GD-AlMg8(Cu) | 17120 | St37-3 | 17405 | RSi48 | 8556-1 | 299 |
1725-1 | GD-AlMg9 | 17120 | St44-2 | 17410 | AlNiCo12/6 | 8556-1 | 30 |
1725-1 | GD-AlSi10Mg | 17120 | St44-3 | 17410 | AlNiCo18/9 | 8556-1 | X10CrNi309 |
1725-1 | GD-AlSi12 | 17120 | St52-3 | 17410 | AlNiCo26/6 | 8556-1 | X12CrNi2212 |
1725-1 | GD-AlSi12(Cu) | 17120 | USt37-2 | 17410 | AlNiCo3/5p | 8556-1 | X12CrNi254 |
1725-1 | GD-AlSi9Cu3 | 17121 | RSt37-2 | 17410 | AlNiCo30/10 | 8556-1 | X12CrNiMo1910 |
1725-1 | GF-AlCu4TiMg | 17121 | St37-3 | 17410 | AlNiCo30/14 | 8556-1 | X15CrNiMn188 |
1725-1 | GF-AlMg3 | 17121 | St44-2 | 17410 | AlNiCo35/5 | 8556-1 | X20CrMo171 |
1725-1 | GF-AlMg3Si | 17121 | St44-3 | 17410 | AlNiCo44/5 | 8556-1 | X20NiCr3618 |
1725-1 | GF-AlSi7Mg | 17121 | St52-3 | 17410 | AlNiCo5/6p | 8556-1 | X2CrNi199 |
1725-1 | GK-AlCu4Ti | 17122 | StSchStr | 17410 | AlNiCo52/6 | 8556-1 | X2CrNi2412 |
1725-1 | GK-AlCu4TiMg | 17123 | EStE255 | 17410 | AlNiCo60/11 | 8556-1 | X2CrNiMnMoN2016 |
1725-1 | GK-AlMg3 | 17123 | EStE285 | 17410 | AlNiCo7/8p | 8556-1 | X2CrNiMo1815 |
1725-1 | GK-AlMg3Si | 17123 | EStE355 | 17410 | AlNiCo9/5 | 8556-1 | X2CrNiMo1816 |
1725-1 | GK-AlMg5 | 17123 | EStE420 | 17410 | FeCoVCr11/12 | 8556-1 | X2CrNiMo1912 |
1725-1 | GK-AlMg5Si | 17123 | EStE460 | 17410 | FeCoVCr4/1 | 8556-1 | X2CrNiMoCu2025 |
1725-1 | GK-AlSi10Mg | 17123 | StE255 | 17410 | Hartferrit 1/18p | 8556-1 | X2CrNiNb2412 |
1725-1 | GK-AlSi10Mg(Cu) | 17123 | StE285 | 17410 | Hartferrit 20/19 | 8556-1 | X3CrNi134 |
1725-1 | GK-AlSi11 | 17123 | StE355 | 17410 | Hartferrit 20/28 | 8556-1 | X5CrNi199 |
1725-1 | GK-AlSi12 | 17123 | StE420 | 17410 | Hartferrit 24/23 | 8556-1 | X5CrNiMo1911 |
1725-1 | GK-AlSi12(Cu) | 17123 | StE460 | 17410 | Hartferrit 25/14 | 8556-1 | X5CrNiMoNb1912 |
1725-1 | GK-AlSi12CuNiMg | 17123 | TStE255 | 17410 | Hartferrit 25/25 | 8556-1 | X5CrNiNb199 |
1725-1 | GK-AlSi5Mg | 17123 | TStE285 | 17410 | Hartferrit 3/18p | 8556-1 | X8Cr14 |
1725-1 | GK-AlSi6Cu4 | 17123 | TStE355 | 17410 | Hartferrit 7/21 | 8556-1 | X8Cr30 |
1725-1 | GK-AlSi7Mg | 17123 | TStE420 | 17410 | Hartferrit 9/19p | 8556-1 | X8CrNi131 |
1725-1 | GK-AlSi9Cu3 | 17123 | TStE460 | 17410 | PtCo60/40 | 8556-1 | X8CrNiMo2313 |
1725-1 | GK-AlSi9Mg | 17124 | EStE255 | 17410 | SeCo112/100 | 8556-1 | X8CrTi18 |
1725-2 | G-AlCu4Tita | 17124 | EStE285 | 17440 | X10Cr13 | 8557-1 | S1 |
1725-2 | G-AlCu4Tiwa | 17124 | EStE355 | 17440 | X10CrNiS189 | 8557-1 | S1Si |
1725-2 | G-AlMg10 | 17124 | EStE420 | 17440 | X12CrMoS17 | 8557-1 | S2 |
1725-2 | G-AlMg10ho | 17124 | EStE460 | 17440 | X15Cr13 | 8557-1 | S2Mo |
1725-2 | G-AlMg3 | 17124 | StE255 | 17440 | X20Cr13 | 8557-1 | S2Ni1 |
1725-2 | G-AlMg3(Cu) | 17124 | StE285 | 17440 | X20CrNi172 | 8557-1 | S2Ni2 |
1725-2 | G-AlSi10Mg(Cu)wa | 17124 | StE355 | 17440 | X2CrNi1911 | 8557-1 | S2Si |
1725-2 | G-AlSi12Mg | 17124 | StE420 | 17440 | X2CrNiMo17132 | 8557-1 | S3 |
1725-2 | G-AlSi5Mgka | 17124 | StE460 | 17440 | X2CrNiMo18143 | 8557-1 | S3Mo |
1725-2 | G-AlSi5Mgwa | 17124 | TStE255 | 17440 | X2CrNiMo18164 | 8557-1 | S4 |
1725-2 | G-AlSi7Mgwa | 17124 | TStE285 | 17440 | X2CrNiMoN17122 | 8557-1 | S4Mo |
1725-2 | G-AlSi9Mg | 17124 | TStE355 | 17440 | X2CrNiMoN17133 | 8557-1 | S6 |
1725-2 | G-AlSi9Mgwa | 17124 | TStE420 | 17440 | X2CrNiMoN17135 | 8560 | 105Cr4 |
1725-2 | GD-AlSi10Mg(Cu) | 17124 | TStE460 | 17440 | X2CrNiN1810 | 8566-1 | 110MnCrTi8 |
1725-2 | GD-AlSi6Cu4 | 17125 | EStE255 | 17440 | X30Cr13 | 8566-1 | 3NiMoCr1220 |
1725-2 | GK-AlCu4Tita | 17125 | EStE285 | 17440 | X38Cr13 | 8566-1 | X35Cr14 |
1725-2 | GK-AlCu4Tiwa | 17125 | EStE355 | 17440 | X45CrMoV15 | 8566-2 | 110MnCrTi8 |
1725-2 | GK-AlMg3Siwa | 17125 | EStE420 | 17440 | X46Cr13 | 8575 | 10MnMo45 |
1725-2 | GK-AlSi10Mg(Cu)wa | 17125 | EStE460 | 17440 | X4CrMoS18 | 8575 | 10MnMoCrV47 |
1725-2 | GK-AlSi10Mgwa | 17125 | StE255 | 17440 | X5CrNi1810 | 8575 | X23CrMoV121 |
1725-2 | GK-AlSi12g | 17125 | StE285 | 17440 | X5CrNi1812 | 8575 | X24CrMoV121 |
1725-2 | GK-AlSi5Mgka | 17125 | StE355 | 17440 | X5CrNiMo17122 | EN 10016-2 | C10D |
1725-2 | GK-AlSi5Mgwa | 17125 | StE420 | 17440 | X5CrNiMo17133 | EN 10016-2 | C12D |
1725-2 | GK-AlSi7Mgwa | 17125 | StE460 | 17440 | X6Cr13 | EN 10016-2 | C15D |
1725-2 | GK-AlSi8Cu3 | 17125 | TStE255 | 17440 | X6Cr17 | EN 10016-2 | C18D |
1725-2 | GK-AlSi9Mgwa | 17125 | TStE285 | 17440 | X6CrAl13 | EN 10016-2 | C20D |
1725-3 | V-AlB3 | 17125 | TStE355 | 17440 | X6CrNiMoNb17122 | EN 10016-2 | C26D |
1725-3 | V-AlB4 | 17125 | TStE420 | 17440 | X6CrNiMoTi17122 | EN 10016-2 | C32D |
1725-3 | V-AlBe5 | 17125 | TStE460 | 17440 | X6CrNiNb1810 | EN 10016-2 | C38D |
1725-3 | V-AlCr5 | 17135 | ASt35 | 17440 | X6CrNiTi1810 | EN 10016-2 | C42D |
1725-3 | V-AlCu50 | 17135 | ASt41 | 17440 | X6CrTi17 | EN 10016-2 | C48D |
1725-3 | V-AlFe5 | 17135 | ASt45 | 17441 | X10Cr13 | EN 10016-2 | C4D |
1725-3 | V-AlMn10 | 17135 | ASt52 | 17441 | X15Cr13 | EN 10016-2 | C50D |
1725-3 | V-AlSi12 | 17140-1 | D10-2 | 17441 | X20Cr13 | EN 10016-2 | C52D |
1725-3 | V-AlSi20 | 17140-1 | D15-2 | 17441 | X2CrNi1911 | EN 10016-2 | C56D |
1725-3 | V-AlTi10 | 17140-1 | D20-2 | 17441 | X2CrNiMo17132 | EN 10016-2 | C58D |
1725-3 | V-AlTi5 | 17140-1 | D25-2 | 17441 | X2CrNiMo18143 | EN 10016-2 | C60D |
1725-3 | V-AlTi5B1 | 17140-1 | D30-2 | 17441 | X2CrNiMo18164 | EN 10016-2 | C62D |
1725-3 | V-AlZr6 | 17140-1 | D35-2 | 17441 | X2CrNiMoN17122 | EN 10016-2 | C66D |
1725-3 | VR-AlSi20 | 17140-1 | D40-2 | 17441 | X2CrNiMoN17133 | EN 10016-2 | C68D |
1725-5 | GB-AlCu4Ti | 17140-1 | D45-2 | 17441 | X2CrNiMoN17135 | EN 10016-2 | C70D |
1725-5 | GB-AlCu4TiMg | 17140-1 | D50-2 | 17441 | X2CrNiN1810 | EN 10016-2 | C72D |
1725-5 | GB-AlMg3 | 17140-1 | D5-2 | 17441 | X30Cr13 | EN 10016-2 | C76D |
1725-5 | GB-AlMg3(Cu) | 17140-1 | D53-2 | 17441 | X38Cr13 | EN 10016-2 | C78D |
1725-5 | GB-AlMg3Si | 17140-1 | D55-2 | 17441 | X45CrMoV15 | EN 10016-2 | C7D |
1725-5 | GB-AlMg5 | 17140-1 | D58-2 | 17441 | X46Cr13 | EN 10016-2 | C80D |
1725-5 | GB-AlMg5Si | 17140-1 | D60-2 | 17441 | X5CrNi1810 | EN 10016-2 | C82D |
1725-5 | GB-AlMg8(Cu) | 17140-1 | D6-2 | 17441 | X5CrNi1812 | EN 10016-2 | C86D |
1725-5 | GB-AlMg9 | 17140-1 | D63-2 | 17441 | X5CrNiMo17122 | EN 10016-2 | C88D |
1725-5 | GB-AlSi10Mg | 17140-1 | D65-2 | 17441 | X5CrNiMo17133 | EN 10016-2 | C92D |
1725-5 | GB-AlSi10Mg(Cu) | 17140-1 | D68-2 | 17441 | X6Cr13 | EN 10016-2 | C9D |
1725-5 | GB-AlSi11 | 17140-1 | D70-2 | 17441 | X6Cr17 | EN 10016-3 | C2D1 |
1725-5 | GB-AlSi12 | 17140-1 | D73-2 | 17441 | X6CrAl13 | EN 10016-3 | C3D1 |
1725-5 | GB-AlSi12(Cu) | 17140-1 | D75-2 | 17441 | X6CrMo171 | EN 10016-3 | C4D1 |
1725-5 | GB-AlSi12CuNiMg | 17140-1 | D78-2 | 17441 | X6CrNb17 | EN 10016-4 | C10D2 |
1725-5 | GB-AlSi5Mg | 17140-1 | D80-2 | 17441 | X6CrNiMoTi17122 | EN 10016-4 | C12D2 |
1725-5 | GB-AlSi6Cu4 | 17140-1 | D8-2 | 17441 | X6CrNiNb1810 | EN 10016-4 | C15D2 |
1725-5 | GB-AlSi7Mg | 17140-1 | D83-2 | 17441 | X6CrNiTi1810 | EN 10016-4 | C18D2 |
1725-5 | GB-AlSi9Cu3 | 17140-1 | D85-2 | 17441 | X6CrTi12 | EN 10016-4 | C20D2 |
1725-5 | GB-AlSi9Mg | 17140-1 | D88-2 | 17441 | X6CrTi17 | EN 10016-4 | C26D2 |
1725-5 | GBD-AlMg8(Cu) | 17140-1 | D9 | 17442 | G-X20CrMo13 | EN 10016-4 | C32D2 |
1725-5 | GBD-AlMg9 | 17140-1 | D95-2 | 17442 | G-X35CrMo17 | EN 10016-4 | C36D2 |
1725-5 | GBD-AlSi10Mg | 17140-2 | 49CrV42 | 17442 | X20Cr13 | EN 10016-4 | C38D2 |
1725-5 | GBD-AlSi12 | 17140-2 | 55SiCr63 | 17442 | X38CrMoV15 | EN 10016-4 | C3D2 |
1725-5 | GBD-AlSi12(Cu) | 17140-2 | 67CrV2 | 17443 | X2CrNiMnMoN22136 | EN 10016-4 | C40D2 |
1725-5 | GBD-AlSi9Cu3 | 17140-2 | 67CrV22 | 17443 | X2CrNiMo18153 | EN 10016-4 | C42D2 |
1732-1 | EL-Al99.5 | 17140-2 | 67SiCr52 | 17443 | X2CrNiMoN18133 | EN 10016-4 | C46D2 |
1732-1 | EL-Al99.5Ti | 17140-2 | VD66-3 | 17443 | X2CrNiMoN18154 | EN 10016-4 | C48D2 |
1732-1 | EL-Al99.8 | 17140-2 | VD71-3 | 17445 | GX12Cr12 | EN 10016-4 | C50D2 |
1732-1 | EL-AlMn1 | 17145 | 10MnMo45 | 17445 | GX1NiCrMoCu25-20-5 | EN 10016-4 | C52D2 |
1732-1 | EL-AlSi12 | 17145 | 10MnSi5 | 17445 | GX1NiCrMoCuN25-20-6 | EN 10016-4 | C56D2 |
1732-1 | EL-AlSi5 | 17145 | 10MnSi7 | 17445 | GX2CrNi19-11 | EN 10016-4 | C58D2 |
1732-1 | S-AlSi5 | 17145 | 11CrMo45 | 17445 | GX2CrNiMo19-11-2 | EN 10016-4 | C5D2 |
1732-1 | SG-Al99.5 | 17145 | 11CrMo55 | 17445 | GX2CrNiMoCuN25-6-3-3 | EN 10016-4 | C60D2 |
1732-1 | SG-Al99.5Ti | 17145 | 11Mn4Al | 17445 | GX2CrNiMoN17-13-4 | EN 10016-4 | C62D2 |
1732-1 | SG-Al99.8 | 17145 | 11Mn4Si | 17445 | GX2CrNiMoN20-18-6 | EN 10016-4 | C66D2 |
1732-1 | SG-AlMg2.7Mn | 17145 | 11MnMo45 | 17445 | GX2CrNiMoN22-5-3 | EN 10016-4 | C68D2 |
1732-1 | SG-AlMg2.7MnZr | 17145 | 11MnSi6 | 17445 | GX2CrNiMoN25-6-3 | EN 10016-4 | C70D2 |
1732-1 | SG-AlMg2Mn0.8 | 17145 | 11NiMn54 | 17445 | GX2CrNiMoN25-7-3 | EN 10016-4 | C72D2 |
1732-1 | SG-AlMg2Mn0.8Zr | 17145 | 11NiMn94 | 17445 | GX2CrNiMoN26-7-4 | EN 10016-4 | C76D2 |
1732-1 | SG-AlMg3 | 17145 | 12CrMo1110 | 17445 | GX2NiCrMo28-20-2 | EN 10016-4 | C78D2 |
1732-1 | SG-AlMg4.5Mn | 17145 | 12Mn6 | 17445 | GX2NiCrMoCuN29-25-5 | EN 10016-4 | C80D2 |
1732-1 | SG-AlMg4.5MnZr | 17145 | 12Mn8 | 17445 | GX2NiCrMoN25-20-5 | EN 10016-4 | C82D2 |
1732-1 | SG-AlMg5 | 17145 | 13Mn12 | 17445 | GX4CrNi13-4 | EN 10016-4 | C86D2 |
1732-1 | SG-AlMn1 | 17145 | 13Mn6 | 17445 | GX4CrNiMo16-5-1 | EN 10016-4 | C88D2 |
1732-1 | SG-AlSi10Mg | 17145 | 13MnMo65 | 17445 | GX4CrNiMo16-5-2 | EN 10016-4 | C8D2 |
1732-1 | SG-AlSi12 | 17145 | 13MnMo85 | 17445 | GX4NiCrCuMo30-20-4 | EN 10016-4 | C92D2 |
1732-1 | SG-AlSi5 | 17145 | 17MnNi4 | 17445 | GX5CrNi19-10 | EN 10016-4 | C98D2 |
1736 | NiCu30MnTi | 17145 | 6CrMo910 | 17445 | GX5CrNiCu16-4 | EN 10025 | E295 |
1736 | NiMo15Cr | 17145 | 7CrMo1110 | 17445 | GX5CrNiMo19-11-2 | EN 10025 | E335 |
1736 | NiMo16Cr | 17145 | 9MnNi4 | 17445 | GX5CrNiMo19-11-3 | EN 10025 | E360 |
1736 | S-NiCr15FeMn | 17145 | RRSD10 | 17445 | GX5CrNiMoNb19-11-2 | EN 10025 | S185 |
1736 | S-NiCr15FeNb | 17145 | RSD10Si | 17445 | GX5CrNiNb19-11 | EN 10025 | S235J2G3 |
1736 | S-NiCr15FeTi | 17145 | RSD7 | 17445 | GX6CrNiN26-7 | EN 10025 | S235J2G4 |
1736 | S-NiCr20 | 17145 | USD5 | 17445 | GX7CrNiMo12-1 | EN 10025 | S235JO |
1736 | S-NiCr20Nb | 17145 | USD6 | 17455 | X2CrNi1911 | EN 10025 | S235JR |
1736 | S-NiCr21Mo9Nb | 17145 | USD7 | 17455 | X2CrNiMo17132 | EN 10025 | S235JRG1 |
1736 | S-NiCu30Al | 17145 | X10CrNi309 | 17455 | X2CrNiMo18143 | EN 10025 | S235JRG2 |
1736 | S-NiCu30Mn | 17145 | X110Mn14 | 17455 | X2CrNiMoN17133 | EN 10025 | S275J2G3 |
1736 | S-NiMn30 | 17145 | X11CrMo61 | 17455 | X2CrNiMoN17135 | EN 10025 | S275J2G4 |
1736 | S-NiMo28 | 17145 | X12CrNi2212 | 17455 | X2CrNiN1810 | EN 10025 | S275JO |
1736 | S-NiTi3 | 17145 | X12CrNi2520 | 17455 | X5CrNi1810 | EN 10025 | S275JR |
1736 | S-NiTi4 | 17145 | X12CrNi265 | 17455 | X5CrNiMo17122 | EN 10025 | S355J2G3 |
17470 | NiCr8010 | 17145 | X15CrNiMn188 | 17455 | X5CrNiMo17133 | EN 10025 | S355J2G4 |
17641 | Pb(Sb) | 17145 | X23CrMoV121 | 17455 | X6Cr17 | EN 10025 | S355JO |
17641 | PbSb5 | 17145 | X24CrMoV121 | 17455 | X6CrNiMoTi17122 | EN 10025 | S355JR |
17641 | PbSb8 | 17145 | X2CrNi199 | 17455 | X6CrNiNb1810 | EN 10025 | S355K2G3 |
17641 | PbSb9 | 17145 | X2CrNiMnMoN2016 | 17455 | X6CrNiTi1810 | EN 10025 | S355K2G4 |
17641 | PbSb9X | 17145 | X2CrNiMo1814 | 17455 | X6CrTi12 | EN 10028-2 | 10CrMo9-10 |
17641 | PbSbAs | 17145 | X2CrNiMo1912 | 17455 | X6CrTi17 | EN 10028-2 | 11CrMo9-10 |
17641 | R-Pb | 17145 | X3CrNi134 | 17456 | X10Cr13 | EN 10028-2 | 13CrMo45 |
17656 | GB-CuAl10Fe | 17145 | X45CrSi93 | 17456 | X2CrNi1911 | EN 10028-2 | 16Mo3 |
17656 | GB-CuAl10Ni | 17145 | X5CrNi199 | 17456 | X2CrNiMo17132 | EN 10028-2 | P235GH |
17656 | GB-CuAl11Ni | 17145 | X5CrNiMo1911 | 17456 | X2CrNiMo18143 | EN 10028-2 | P265GH |
17656 | GB-CuPb10Sn | 17145 | X5CrNiMoNb1912 | 17456 | X2CrNiMoN17133 | EN 10028-2 | P295GH |
17656 | GB-CuPb15Sn | 17145 | X5CrNiNb199 | 17456 | X2CrNiMoN17135 | EN 10028-2 | P355GH |
17656 | GB-CuPb20Sn | 17145 | X7CrMo61 | 17456 | X2CrNiN1810 | EN 10028-3 | P275N |
17656 | GB-CuSn10 | 17145 | X7CrMo91 | 17456 | X5CrNi1810 | EN 10028-3 | P275NH |
17656 | GB-CuSn10Zn | 17145 | X8Cr14 | 17456 | X5CrNiMo17122 | EN 10028-3 | P275NL1 |
17656 | GB-CuSn12 | 17145 | X8Cr30 | 17456 | X5CrNiMo17133 | EN 10028-3 | P275NL2 |
17656 | GB-CuSn12Ni | 17145 | X8CrTi18 | 17456 | X6Cr17 | EN 10028-3 | P355N |
17656 | GB-CuSn12Pb | 1715-1 | CoNiCr2620 | 17456 | X6CrAl13 | EN 10028-3 | P355NH |
17656 | GB-CuSn5ZnPb | 1715-1 | MnCuNi | 17456 | X6CrNiMoTi17122 | EN 10028-3 | P355NL1 |
17656 | GB-CuSn6ZnNi | 1715-1 | Ni36 | 17456 | X6CrNiNb1810 | EN 10028-3 | P355NL2 |
17656 | GB-CuSn7ZnPb | 1715-1 | Ni42 | 17456 | X6CrNiTi1810 | EN 10028-3 | P460N |
17656 | GB-CuZn15Si14 | 1715-1 | Ni46 | 17456 | X6CrTi12 | EN 10028-3 | P460NH |
17656 | GB-CuZn25A15 | 1715-1 | NiCr1611 | 17456 | X6CrTi17 | EN 10028-3 | P460NL1 |
17656 | GB-CuZn33Pb | 1715-1 | NiMn206 | 17457 | X2CrNi1911 | EN 10028-3 | P460NL2 |
17656 | GB-CuZn34Al2 | 1715-1 | X60NiMn147 | 17457 | X2CrNiMo17132 | EN 10028-4 | 11MnNi5-3 |
17656 | GB-CuZn35Al1 | 17172 | RRStE210.7 | 17457 | X2CrNiMo18143 | EN 10028-4 | 12Ni14 |
17656 | GB-CuZn37Pb | 17172 | RRStE240.7 | 17457 | X2CrNiMoN17133 | EN 10028-4 | 12Ni19 |
17656 | GB-CuZn39Pb | 17172 | StE210.7 | 17457 | X2CrNiMoN17135 | EN 10028-4 | 13MnNi6-3 |
17658 | G-CuNi10 | 17172 | StE240.7 | 17457 | X2CrNiN1810 | EN 10028-4 | 15NiMn6 |
17658 | G-CuNi30 | 17172 | StE290.7 | 17457 | X5CrNi1810 | EN 10028-4 | X7Ni9 |
17740 | L-CNi99.6 | 17172 | StE290.7TM | 17457 | X5CrNiMo17122 | EN 10028-4 | X8Ni9 |
17740 | LC-Ni99 | 17172 | StE320.7 | 17457 | X5CrNiMo17133 | EN 10028-6 | P460Q |
17740 | Ni99.2 | 17172 | StE320.7TM | 17457 | X6CrNiMoTi17122 | EN 10028-6 | P460QH |
17740 | Ni99.4Fe | 17172 | StE360.7 | 17457 | X6CrNiNb1810 | EN 10028-6 | P460QL |
17740 | Ni99.6 | 17172 | StE360.7TM | 17457 | X6CrNiTi1810 | EN 10028-6 | P500Q |
17740 | Ni99.7 | 17172 | StE385.7 | 17458 | X2CrNi1911 | EN 10028-6 | P500QH |
17740 | Ni99.7Mg0.05 | 17172 | StE385.7TM | 17458 | X2CrNiMo17132 | EN 10028-6 | P500QL |
17740 | Ni99.7Mg0.07 | 17172 | StE415.7 | 17458 | X2CrNiMo18143 | EN 10028-6 | P550Q |
17740 | Ni99.8 | 17172 | StE415.7TM | 17458 | X2CrNiMoN17133 | EN 10028-6 | P550QH |
17740 | Ni99.8Mg | 17172 | StE445.7TM | 17458 | X2CrNiMoN17135 | EN 10028-6 | P550QL |
17741 | NiMn1 | 17172 | StE480.7TM | 17458 | X2CrNiN1810 | EN 10028-6 | P690Q |
17741 | NiMn1C | 17173 | 10Ni14 | 17458 | X5CrNi1810 | EN 10028-6 | P690QH |
17741 | NiMn2 | 17173 | 11MnNi53 | 17458 | X5CrNiMo17122 | EN 10028-6 | P690QL |
17741 | NiMn3Al | 17173 | 12Ni19 | 17458 | X5CrNiMo17133 | EN 10083-1 | 25CrMo4 |
17741 | NiMn5 | 17173 | 13MnNi63 | 17458 | X6CrNiMoNb17122 | EN 10083-1 | 25CrMoS4 |
17742 | LC-NiCr15Fe | 17173 | 26CrMo4 | 17458 | X6CrNiMoTi17122 | EN 10083-1 | 28Mn6 |
17742 | NiCr10 | 17173 | TTSt35N | 17458 | X6CrNiNb1810 | EN 10083-1 | 30CrNiMo8 |
17742 | NiCr15Fe | 17173 | TTSt35V | 17458 | X6CrNiTi1810 | EN 10083-1 | 34Cr4 |
17742 | NiCr20AlSi | 17173 | X8Ni9 | 17459 | X3CrNiMoN1713 | EN 10083-1 | 34CrMo4 |
17742 | NiCr20Ti | 17174 | 10Ni14 | 17459 | X3CrNiN1811 | EN 10083-1 | 34CrMoS4 |
17742 | NiCr20TiAl | 17174 | 11MnNi53 | 17459 | X5NiCrAlTi3120 | EN 10083-1 | 34CrNiMo6 |
17742 | NiCr6015 | 17174 | 12Ni19 | 17459 | X6CrNi1811 | EN 10083-1 | 34CrS4 |
17742 | NiMo16Cr | 17174 | 13MnNi63 | 17459 | X6CrNiMo1713 | EN 10083-1 | 36CrNiMo4 |
17743 | NiCu30Al | 17174 | TTSt35N | 17459 | X8CrNiMoNb1616 | EN 10083-1 | 36NiCrMo16 |
17743 | NiCu30Fe | 17174 | TTSt35V | 17459 | X8CrNiMoVNb1613 | EN 10083-1 | 37Cr4 |
17744 | NiCr20Co18Ti | 17174 | X8Ni9 | 17459 | X8CrNiNb1613 | EN 10083-1 | 37CrS4 |
17744 | NiCr20Mo15 | 17175 | 10CrMo910 | 17459 | X8CrNiTi1810 | EN 10083-1 | 38Cr2 |
17744 | NiCr21Mo | 17175 | 13CrMo44 | 17459 | X8NiCrAlTi3221 | EN 10083-1 | 38CrS2 |
17744 | NiMo | 17175 | 14MoV63 | 17460 | X3CrNiMoN1713 | EN 10083-1 | 41Cr4 |
17745 | Ni42 | 17175 | 15Mo3 | 17460 | X3CrNiN1811 | EN 10083-1 | 41CrS4 |
17745 | Ni45 | 17175 | 17Mn4 | 17460 | X5NiCrAlTi3120 | EN 10083-1 | 42CrMo4 |
17745 | Ni48 | 17175 | 19Mn5 | 17460 | X6CrNi1811 | EN 10083-1 | 42CrMoS4 |
17745 | Ni49 | 17175 | St35.8 | 17460 | X6CrNiMo1713 | EN 10083-1 | 46Cr2 |
17745 | NiCo2823 | 17175 | St45.8 | 17460 | X8CrNiMoNb1616 | EN 10083-1 | 46CrS2 |
17745 | NiCo2918 | 17175 | X20CrMoV121 | 17460 | X8CrNiMoVNb1613 | EN 10083-1 | 50CrMo4 |
17745 | NiFe15Mo | 17176 | 10CrMo910 | 17460 | X8CrNiNb1613 | EN 10083-1 | 51CrV4 |
17745 | NiFe16CuMo | 17176 | 12CrMo1210 | 17460 | X8CrNiTi1810 | EN 10083-1 | C22E |
17745 | NiFe1CuCr | 17176 | 12CrMo195 | 17460 | X8NiCrAlTi3221 | EN 10083-1 | C22R |
17745 | NiFe44 | 17176 | 12CrMo910 | 17465 | G-CoCr28 | EN 10083-1 | C25E |
17745 | NiFe46 | 17176 | 13CrMo44 | 17465 | G-NiCr28W | EN 10083-1 | C25R |
17745 | NiFe47 | 17176 | 20CrMoV135 | 17465 | G-X25CrNiSi18-9 | EN 10083-1 | C30E |
17745 | NiFe47Cr | 17176 | 25CrMo4 | 17465 | G-X25CrNiSi20-14 | EN 10083-1 | C30R |
17745 | NiFe48Cr | 17176 | X12CrMo91 | 17465 | G-X30CrNiSiNb24-24 | EN 10083-1 | C35E |
17800 | H-Mg99.8 | 17176 | X20CrMoV121 | 17465 | G-X30CrSi6 | EN 10083-1 | C35R |
17800 | H-Mg99.95 | 17177 | 15Mo3 | 17465 | G-X40CrNiSi22-9 | EN 10083-1 | C40E |
17810 | SnSb2Cu1.5 | 17177 | St37.8 | 17465 | G-X40CrNiSi25-12 | EN 10083-1 | C40R |
17810 | SnSb5Cu1.5 | 17177 | St42.8 | 17465 | G-X40CrNiSi25-20 | EN 10083-1 | C45E |
17850 | 3.7025 | 17178 | EStE255 | 17465 | G-X40CrNiSi27-4 | EN 10083-1 | C45R |
17850 | 3.7035 | 17178 | EStE285 | 17465 | G-X40CrSi13 | EN 10083-1 | C50E |
17850 | 3.7055 | 17178 | EStE355 | 17465 | G-X40CrSi17 | EN 10083-1 | C50R |
17850 | 3.7065 | 17178 | EStE420 | 17465 | G-X40CrSi23 | EN 10083-1 | C55E |
17851 | TiAl5Sn2 | 17178 | EStE460 | 17465 | G-X40CrSi29 | EN 10083-1 | C55R |
17851 | TiAl6V4 | 17178 | StE255 | 17465 | G-X40NiCrSi35-25 | EN 10083-1 | C60E |
40501-1 | E-AlF10 | 17178 | StE285 | 17465 | G-X40NiCrSi38-18 | EN 10083-1 | C60R |
40501-1 | E-AlF13 | 17178 | StE355 | 17465 | G-X40NiCrSiNb35-25 | EN 10083-2 | C22 |
40501-1 | E-AlF16 | 17178 | StE420 | 17465 | G-X40NiCrSiNb38-18 | EN 10083-2 | C25 |
40501-1 | E-AlF7 | 17178 | StE460 | 17470 | CrAl144 | EN 10083-2 | C30 |
40501-2 | E-AlF10 | 17178 | TStE255 | 17470 | CrAl205 | EN 10083-2 | C35 |
40501-2 | E-AlF7 | 17178 | TStE285 | 17470 | CrAl255 | EN 10083-2 | C40 |
40501-2 | E-AlMgSi0.5F22 | 17178 | TStE355 | 17470 | CrNi2520 | EN 10083-2 | C45 |
40501-3 | E-AlF10 | 17178 | TStE420 | 17470 | NiCr3020 | EN 10083-2 | C50 |
40501-3 | E-AlF13 | 17178 | TStE460 | 17470 | NiCr6015 | EN 10083-2 | C55 |
40501-3 | E-AlF6.5 | 17178 | WStE255 | 17470 | NiCr7030 | EN 10083-2 | C60 |
40501-3 | E-AlF8 | 17178 | WStE285 | 17470 | NiCr8020 | EN 10083-3 | 20MnB5 |
40501-3 | E-AlMgSi0.5F17 | 17178 | WStE355 | 17471 | CuMn12Ni | EN 10083-3 | 27MnCrB5-2 |
40501-3 | E-AlMgSi0.5F22 | 17178 | WStE420 | 17471 | CuMn12niAl | EN 10083-3 | 30MnB5 |
40501-3 | E-Alp | 17178 | WStE460 | 17471 | CuMn3 | EN 10083-3 | 33MnCrB5-2 |
40501-4 | E-AlF17 | 17179 | EStE255 | 17471 | CuNi10 | EN 10083-3 | 38MnB5 |
40501-4 | E-AlF7 | 17179 | EStE285 | 17471 | CuNi2 | EN 10083-3 | 39MnCrB6-2 |
40501-4 | E-AlF9 | 17179 | EStE355 | 17471 | CuNi23Mn | EN 10113-2 | S275N |
8512 | L-AlSi12 | 17179 | EStE420 | 17471 | CuNi30Mn | EN 10113-2 | S275NL |
8512 | L-AlSiSn | 17179 | EStE460 | 17471 | CuNi44 | EN 10113-2 | S355N |
8512 | L-ZnCd40 | 17179 | StE255 | 17471 | CuNi6 | EN 10113-2 | S355NL |
8513-3 | L-AlSi10 | 17179 | StE285 | 17471 | NiCr20AlSi | EN 10113-2 | S420N |
8513-3 | L-AlSi12 | 17179 | StE355 | 17471 | NiCr6015 | EN 10113-2 | S420NL |
8513-3 | L-AlSi7.5 | 17179 | StE420 | 17471 | NiCr8020 | EN 10113-2 | S460N |
ISO 1494-4 | AlSn20Cu | 17179 | StE460 | 17480 | NiCr20TiAl | EN 10113-2 | S460NL |
ISO 1494-4 | AlSn6CuNi | 17179 | TStE255 | 17480 | NiFe25Cr20NbTi | EN 10113-3 | S275M |
ISO 4381 | AlCd3CuNi | 17179 | TStE285 | 17480 | X45CrNiW189 | EN 10113-3 | S275ML |
ISO 4381 | AlSi4Cd | 17179 | TStE355 | 17480 | X45CrSi93 | EN 10113-3 | S355M |
ISO 4381 | AlSn20Cu | 17179 | TStE420 | 17480 | X50CrMnNiNbN219 | EN 10113-3 | S355ML |
ISO 4381 | AlSn6CuNi | 17179 | TStE460 | 17480 | X53CrMnNiN219 | EN 10113-3 | S420M |
ISO 6297 | AlSn6CuNi | 17179 | WStE255 | 17480 | X55CrMnNiN208 | EN 10113-3 | S420ML |
1614-1 | RRSt23 | 17179 | WStE285 | 17480 | X60CrMnMoVNbN2110 | EN 10113-3 | S460M |
1614-1 | St22 | 17179 | WStE355 | 17480 | X85CrMoV182 | EN 10113-3 | S460ML |
1614-1 | St24 | 17179 | WStE420 | 17730 | G-Ni90Si | EN 10120 | P245NB |
1614-1 | USt23 | 17179 | WStE460 | 17730 | G-Ni93C | EN 10120 | P265NB |
1614-2 | RRStW23 | 17182 | GS-13MnNi64 | 17730 | G-Ni95 | EN 10120 | P310NB |
1614-2 | StW22 | 17182 | GS-16Mn5 | 17730 | G-NiCu30Nb | EN 10120 | P355NB |
1614-2 | StW24 | 17182 | GS-20Mn5 | 17730 | G-NiCu30Si3 | EN 10130 | DC01 |
1614-2 | UStW23 | 17182 | GS-8Mn7 | 17730 | G-NiCu30Si4 | EN 10130 | DC03 |
1615 | St33 | 17182 | GS-8MnMo74 | 17740 | LC-Ni99 | EN 10130 | DC04 |
1623-2 | St37-2G | 17201 | 20MnMoNi45 | 17740 | LC-Ni99.6 | EN 10130 | DC05 |
1623-2 | St37-3G | 17201 | 28Mn6 | 17740 | Ni99.2 | EN 10130 | DC06 |
1623-2 | St44-3G | 17201 | 28NiCrMoV85 | 17740 | Ni99.6 | EN 10139 | DC01 |
1623-2 | St50-2G | 17201 | 30CrMoV9 | 17740 | Ni99.7Mg | EN 10139 | DC03 |
1623-2 | St52-3G | 17201 | 32CrMo12 | 17741 | Ni99.4Fe | EN 10139 | DC04 |
1623-2 | St60-2G | 17201 | 33NiCrMo145 | 17741 | NiMn1 | EN 10139 | DC05 |
1623-2 | St70-2G | 17201 | 50CrMo4 | 17741 | NiMn2 | EN 10139 | DC06 |
1623-2 | USt37-2G | 17201 | Ck22 | 17741 | NiMn3Al | EN 10142 | FeP02G |
1623-3 | ED3 | 17201 | Ck35 | 17741 | NiMn5 | EN 10142 | FeP03G |
1623-3 | ED4 | 17201 | Ck45 | 17742 | LC-NiCr15Fe | EN 10142 | FeP05G |
1623-3 | EK2 | 17201 | Ck53 | 17742 | NiCr15Fe | EN 10142 | FeP06G |
1623-3 | EK4 | 17201 | Ck60 | 17742 | NiCr20AlSi | EN 10147 | S220GD |
1624 | RRSt3 | 17204 | 25CrMo4 | 17742 | NiCr20Ti | EN 10147 | S250GD |
1624 | St2 | 17204 | 28Mn6 | 17742 | NiCr20TiAl | EN 10147 | S280GD |
1624 | St4 | 17204 | 30CrMoV9 | 17742 | NiCr23Fe | EN 10147 | S320GD |
1624 | USt3 | 17204 | 30CrNiMo8 | 17742 | NiCr6015 | EN 10147 | S350GD |
1626 | St37.0 | 17204 | 34CrMo4 | 17742 | NiCr7030 | EN 10147 | S550GD |
1626 | St44.0 | 17204 | 34CrNiMo6 | 17742 | NiCr8020 | EN 10149-2 | S315MC |
1626 | St52.0 | 17204 | 36CrNiMo4 | 17743 | LC-NiCu30Fe | EN 10149-2 | S355MC |
1626 | USt37.0 | 17204 | 36Mn4 | 17743 | NiCu30Al | EN 10149-2 | S420MC |
1628 | St37.4 | 17204 | 36Mn5 | 17743 | NiCu30Fe | EN 10149-2 | S460MC |
1628 | St44.4 | 17204 | 41Cr4 | 17744 | NiCr21Mo | EN 10149-2 | S500MC |
1628 | St52.4 | 17204 | 42CrMo4 | 17744 | NiCr21Mo6Cu | EN 10149-2 | S550MC |
1629 | St37.0 | 17204 | C22 | 17744 | NiCr22Mo6Cu | EN 10149-2 | S600MC |
1629 | St44.0 | 17204 | C22Pb | 17744 | NiCr22Mo7Cu | EN 10149-2 | S650MC |
1629 | St52.0 | 17204 | C35 | 17744 | NiCr22Mo9Nb | EN 10149-2 | S700MC |
1630 | St37.4 | 17204 | C35Pb | 17744 | NiMo16Cr15W | EN 10149-3 | S260NC |
1630 | St44.4 | 17204 | C45 | 17744 | NiMo16Cr16Ti | EN 10149-3 | S315NC |
1630 | St52.4 | 17204 | C45Pb | 17744 | NiMo28 | EN 10149-3 | S355NC |
1651 | 10S20 | 17204 | C55 | 17745 | E3 | EN 10149-3 | S420NC |
1651 | 10SPb20 | 17204 | C55Pb | 17745 | E4 | EN 10152 | DC01+ZE |
1651 | 15S10 | 17204 | C60 | 17745 | F3 | EN 10152 | DC03+ZE |
1651 | 35S20 | 17204 | C60Pb | 17745 | Ni42 | EN 10152 | DC04+ZE |
1651 | 35SPb20 | 17204 | Ck22 | 17745 | Ni49 | EN 10152 | DC05+ZE |
1651 | 45S20 | 17204 | Ck35 | 17745 | NiCo2823 | EN 10152 | DC06+ZE |
1651 | 45SPb20 | 17204 | Ck45 | 17745 | NiCo2918 | EN 10155 | S235J0W |
1651 | 60S20 | 17204 | Ck55 | 17745 | NiFe15Mo | EN 10155 | S235J2W |
1651 | 60SPb20 | 17204 | Ck60 | 17745 | NiFe16CuCr | EN 10155 | S355J0W |
1651 | 9SMn28 | 17204 | Cm22 | 17745 | NiFe16CuMo | EN 10155 | S355J0WP |
1651 | 9SMn36 | 17204 | Cm35 | 17745 | NiFe44 | EN 10155 | S355J2G1W |
1651 | 9SMnPb28 | 17204 | Cm45 | 17745 | NiFe45 | EN 10155 | S355J2G2W |
1651 | 9SMnPb36 | 17204 | Cm55 | 17745 | NiFe46 | EN 10155 | S355J2WP |
1652-2 | RSt37-2 | 17204 | Cm60 | 17745 | NiFe47 | EN 10155 | S355K2G1W |
1652-2 | RZSt37-2 | 17205 | GS-25CrMo4 | 17745 | NiFe47Cr | EN 10155 | S355K2G2W |
1652-2 | St37-2 | 17205 | GS-25CrNiMo4 | 17745 | NiFe48Cr | EN 10203 | DR550 |
1652-2 | St37-3 | 17205 | GS-30CrMoV64 | 17745 | RNi2 | EN 10203 | DR620 |
1652-2 | St44-2 | 17205 | GS-30Mn5 | 17745 | RNi5 | EN 10203 | DR660 |
1652-2 | St44-3 | 17205 | GS-30NiCrMo85 | 21544 | 31Mn4 | EN 10203 | T50 |
1652-2 | St50-2 | 17205 | GS-33NiCrMo744 | 22252 | 23MnNiCrMo52 | EN 10203 | T52 |
1652-2 | St52-3 | 17205 | GS-34CrMo4 | 2391-2 | St30Al | EN 10203 | T57 |
1652-2 | St60-2 | 17205 | GS-34CrNiMo6 | 2391-2 | St30Si | EN 10203 | T61 |
1652-2 | St70-2 | 17205 | GS-35CrMoV104 | 2391-2 | St35 | EN 10203 | T65 |
1652-2 | USt37-2 | 17205 | GS-42CrMo4 | 2391-2 | St45 | EN 10207 | SPH235 |
1652-2 | UZSt37-2 | 17210 | 15CrNi6 | 2391-2 | St52 | EN 10207 | SPH265 |
1652-2 | ZSt37-2 | 17210 | 16MnCr5 | 2393-2 | RSt28 | EN 10207 | SPHL275 |
1652-2 | ZSt37-3 | 17210 | 16MnCrS5 | 2393-2 | RSt34-2 | EN 10208-2 | L245MB |
1652-2 | ZSt44-2 | 17210 | 17Cr3 | 2393-2 | RSt37-2 | EN 10208-2 | L245NB |
1652-2 | ZSt44-3 | 17210 | 17CrNiMo6 | 2393-2 | St28 | EN 10208-2 | L290MB |
1652-2 | ZSt50-2 | 17210 | 20Cr4 | 2393-2 | St34-2 | EN 10208-2 | L290NB |
1652-2 | ZSt52-3 | 17210 | 20CrS4 | 2393-2 | St37-2 | EN 10208-2 | L360MB |
1652-2 | ZSt60-2 | 17210 | 20MnCr5 | 2393-2 | St44-2 | EN 10208-2 | L360NB |
1652-2 | ZSt70-2 | 17210 | 20MnCrS5 | 2393-2 | St52-3 | EN 10208-2 | L360QB |
1652-3 | 15CrNi6 | 17210 | 20MoCr4 | 2393-2 | USt28 | EN 10208-2 | L415MB |
1652-3 | 16MnCr5 | 17210 | 20MoCrS4 | 2393-2 | USt34-2 | EN 10208-2 | L415NB |
1652-3 | 16MnCrS5 | 17210 | 21NiCrMo2 | 2393-2 | USt37-2 | EN 10208-2 | L415QB |
1652-3 | 17Cr3 | 17210 | 21NiCrMoS2 | 2394-2 | RSt28 | EN 10208-2 | L450MB |
1652-3 | 17CrNiMo6 | 17210 | 22CrMoS35 | 2394-2 | RSt34-2 | EN 10208-2 | L450QB |
1652-3 | 20Cr4 | 17210 | C10 | 2394-2 | RSt37-2 | EN 10208-2 | L485MB |
1652-3 | 20CrS4 | 17210 | C10Pb | 2394-2 | St28 | EN 10208-2 | L485QB |
1652-3 | 20MnCr5 | 17210 | C15 | 2394-2 | St34-2 | EN 10208-2 | L555MB |
1652-3 | 20MnCrS5 | 17210 | C15Pb | 2394-2 | St37-2 | EN 10208-2 | L555QB |
1652-3 | 20MoCr4 | 17210 | Ck10 | 2394-2 | St44-2 | EN 10209 | DC01EK |
1652-3 | 20MoCrS4 | 17210 | Ck15 | 2394-2 | St52-3 | EN 10209 | DC03ED |
1652-3 | 21NiCrMo2 | 17210 | Cm15 | 2394-2 | USt28 | EN 10209 | DC04ED |
1652-3 | 21NiCrMoS2 | 17211 | 15CrMoV59 | 2394-2 | USt34-2 | EN 10209 | DC04EK |
1652-3 | 22CrMoS35 | 17211 | 31CrMo12 | 2394-2 | USt37-2 | EN 10209 | DC06ED |
1652-3 | C10 | 17211 | 31CrMoV9 | 2528 | 10CrMo9-10 | EN 10209 | DC06EK |
1652-3 | C15 | 17211 | 34CrAlMo5 | 2528 | 10Ni14 | EN 10210-1 | S235JRH |
1652-3 | Ck10 | 17211 | 34CrAlNi7 | 2528 | 12CrMo195 | EN 10210-1 | S275J0H |
1652-3 | Ck15 | 17212 | 38Cr4 | 2528 | 13CrMo44 | EN 10210-1 | S275J2H |
1652-3 | Cm15 | 17212 | 41CrMo4 | 2528 | 15Mo3 | EN 10210-1 | S275NH |
1652-4 | 25CrMo4 | 17212 | 42Cr4 | 2528 | C21 | EN 10210-1 | S275NLH |
1652-4 | 25CrMoS4 | 17212 | 45Cr2 | 2528 | C22.3 | EN 10210-1 | S355J0H |
1652-4 | 28Cr4 | 17212 | 49CrMo4 | 2528 | C22.8 | EN 10210-1 | S355J2H |
1652-4 | 28CrS4 | 17212 | Cf35 | 2528 | HI | EN 10210-1 | S355NH |
1652-4 | 28Mn6 | 17212 | Cf45 | 2528 | HII | EN 10210-1 | S355NLH |
1652-4 | 30CrMoV9 | 17212 | Cf53 | 2528 | RSt37-2 | EN 10210-1 | S460NH |
1652-4 | 30CrNiMo8 | 17212 | Cf70 | 2528 | St52-3 | EN 10210-1 | S460NLH |
1652-4 | 32Cr2 | 17221 | 38Si7 | 2528 | StE355 | EN 10214 | DX51D+ZA |
1652-4 | 32CrS2 | 17221 | 50CrV4 | 2528 | TStE285 | EN 10214 | DX52D+ZA |
1652-4 | 34Cr4 | 17221 | 51CrMoV4 | 2528 | TStE355 | EN 10214 | DX53D+ZA |
1652-4 | 34CrMo4 | 17221 | 54SiCr6 | 2528 | USt37-2 | EN 10214 | DX54D+ZA |
1652-4 | 34CrMoS4 | 17221 | 55Cr3 | 2528 | WStE355 | EN 10214 | S220GD+ZA |
1652-4 | 34CrNiMo6 | 17221 | 60SiCr7 | 2528 | X2CrNi1911 | EN 10214 | S250GD+ZA |
1652-4 | 34CrS4 | 17222 | 50CrV4 | 2528 | X2CrNiMo17132 | EN 10214 | S280GD+ZA |
1652-4 | 36CrNiMo4 | 17222 | 55Si7 | 2528 | X5CrNi1810 | EN 10214 | S320GD+ZA |
1652-4 | 37Cr4 | 17222 | 67SiCr5 | 2528 | X5CrNiMo17122 | EN 10214 | S350GD+ZA |
1652-4 | 37CrS4 | 17222 | 71Si7 | 2528 | X6CrNiMoTi17122 | EN 10214 | S550GD+ZA |
1652-4 | 38Cr2 | 17222 | C55 | 2528 | X6CrNiTi1810 | EN 10215 | DX51D+AZ |
1652-4 | 38CrS2 | 17222 | C60 | 41301 | A0 | EN 10215 | DX52D+AZ |
1652-4 | 41Cr4 | 17222 | C67 | 41301 | A2 | EN 10215 | DX53D+AZ |
1652-4 | 41CrS4 | 17222 | C75 | 41301 | A3 | EN 10215 | DX54D+AZ |
1652-4 | 42CrMo4 | 17222 | Ck101 | 41301 | C2 | EN 10215 | S250GD+AZ |
1652-4 | 42CrMoS4 | 17222 | Ck55 | 41301 | C5 | EN 10215 | S280GD+AZ |
1652-4 | 46Cr2 | 17222 | Ck60 | 41301 | D1 | EN 10215 | S320GD+AZ |
1652-4 | 46CrS2 | 17222 | Ck67 | 41301 | D1a | EN 10215 | S350GD+AZ |
1652-4 | 50CrMo4 | 17222 | Ck75 | 41301 | D3 | EN 10215 | S550GD+AZ |
1652-4 | 50CrV4 | 17222 | Ck85 | 41301 | E3 | EN 756 | S0 |
1652-4 | C22 | 17223-1 | Federstahldraht A | 41301 | E4 | EN 756 | S1 |
1652-4 | C35 | 17223-1 | Federstahldraht B | 41301 | F3 | EN 756 | S1Mo |
1652-4 | C45 | 17223-1 | Federstahldraht C | 4133 | 15Mo3 | EN 756 | S1Si |
1652-4 | C60 | 17223-1 | Federstahldraht D | 4133 | HII | EN 756 | S2 |
1652-4 | Ck22 | 17223-2 | Federstahldraht FD | 4133 | RSt37-2 | EN 756 | S2Mo |
1652-4 | Ck35 | 17223-2 | Federstahldraht FDCrV | 4133 | St37-2 | EN 756 | S2Ni |
1652-4 | Ck45 | 17223-2 | Federstahldraht FDSiCr | 4133 | St52-3 | EN 756 | S2Ni1,5 |
1652-4 | Ck60 | 17223-2 | Federstahldraht VD | 4133 | USt37-2 | EN 756 | S2Ni1Mo |
1652-4 | Cm22 | 17223-2 | Federstahldraht VDCrV | 4133 | X1CrNiMoTi18132 | EN 756 | S2Ni3 |
1652-4 | Cm35 | 17223-2 | Federstahldraht VDSiCr | 4133 | X1NiCrMoCuN25205 | EN 756 | S2Si |
1652-4 | Cm45 | 17224 | X12CrNi177 | 4133 | X2CrNiMo18143 | EN 756 | S2Si2 |
1652-4 | Cm60 | 17224 | X5CrNiMo1810 | 4133 | X5CrNi1810 | EN 756 | S3 |
1654-2 | QSt32-3 | 17224 | X7CrNiAl177 | 4133 | X6CrNiMoTi17122 | EN 756 | S3Mo |
1654-2 | QSt34-3 | 17230 | 100Cr2 | 4133 | X6CrNiTi1810 | EN 756 | S3Ni1,5 |
1654-2 | QSt36-3 | 17230 | 100Cr6 | 43720 | M2 | EN 756 | S3Ni1,5Mo |
1654-2 | QSt38-3 | 17230 | 100CrMn6 | 43720 | NiCr6015 | EN 756 | S3Ni1Mo |
1654-3 | 15CrNi6 | 17230 | 100CrMnMo8 | 43720 | St35.8 | EN 756 | S3Si |
1654-3 | 16MnCr5 | 17230 | 100CrMo7 | 43720 | X10CrAl18 | EN 756 | S4 |
1654-3 | 17Cr3 | 17230 | 100CrMo73 | 43720 | X10CrAl24 | EN 756 | S4Mo |
1654-3 | 20MoCr4 | 17230 | 16CrNiMo6 | 43720 | X10CrSi18 | EN 756 | S4Si |
1654-3 | 21NiCrMo2 | 17230 | 17MnCr5 | 43720 | X10NiCr3220 | | |
1654-3 | Cq15 | 17230 | 17NiCrMo14 | 43720 | X15CrNiSi2520 | | |
Monday, September 10, 2007
DIN Numbering System
Subscribe to:
Post Comments (Atom)
[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.
Hello, Please see the response below. Regards. P. Goswami, P. Eng, IWE. From: materials-welding@googlegroups.com <materials-weld...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment