Hello friends,
To get RT quality from FCAW in pipe joints what precautions we need to take ?
regards
Ravinder Sharma
Hello friends,
To get RT quality from FCAW in pipe joints what precautions we need to take ?
regards
Ravinder Sharma
Hello, Please see the response below. Regards. P. Goswami, P. Eng, IWE. From: materials-welding@googlegroups.com <materials-weld...